Color, good PP-R water pipe color is soft and uniform, no noise. (PP-R pipes mainly include white, gray, purple, green, yellow, and blue. Consumers often think that white is the best. In fact, color is not the standard for judging quality. In fact, the quality of PP-R pipes is similar to that of PP-R pipes. The color of the water pipe has nothing to do with it. The plastic particles are mainly white and transparent (there are also other colors that have been added with masterbatch), as long as the masterbatch is added, any color can be produced, and the masterbatch will not be decomposed nor will it change the quality of PP-R , so it doesn't matter what color the water pipe is. According to the national regulations, the PP-R water pipe must have good light-blocking performance. In this regard, gray or other opaque properties will be better. But this advantage is only In the installation of open pipes and pipe wells, the water pipes of home improvement are all buried in the dark, so there is no such thing as gray is better than other colors. PP-R pipes are completely opaque, and pseudo PP-R pipes are slightly transparent. Or semi-transparent. White products can only be produced from pure PP-R raw materials. For example, the color of products produced by adding recycled materials, scraps, and scraps is not soft or uniform, while other color products processed with color masterbatch are added and recycled. materials, scraps, scraps, etc. will not affect the color of the product. This is why many manufacturers who focus on quality and home improvement retail are mainly white); The inner and outer surfaces of the product should be smooth and flat, no bubbles, obvious defects such as pits, trenches and impurities.

"touch" texture

Et godt PP-R-vannrør er 100 prosent PP-R-råstoff (uten tilsetningsstoffer). Teksturen er ren, overflaten er glatt og hånden føles myk, og pseudo PP-R-røret føles glatt. Generelt sett er de grove partiklene sannsynligvis blandet med urenheter;

"smell" the smell

Hovedmaterialet i PP-R-røret er polypropylen. Gode ​​rør har ingen lukt, og dårlige rør har en merkelig lukt. Det er sannsynligvis blandet med polyetylen i stedet for polypropylen;

"pinch" hardness

PP-R-rør har betydelig hardhet, og et rør som kan deformeres ved å klemme er definitivt ikke et PP-R-rør;

"Quantity" Wall Thickness

I tillegg kan vernier-kalipere brukes til å måle om veggtykkelsen på røret er opp til standard og jevn. Vanligvis produseres gode rør i strengt samsvar med den nasjonale standarden, men denne metoden krever en viss forståelse av den nasjonale standarden for PP-R-rør.

"listen" to the sound

Lyden av PP-R-røret er matt, og lyden av pseudo-PP-R-røret er skarpere.

"Smash" elasticity

A good PP-R pipe has good "resilience" and is easy to smash. Naturally, it is not a good PP-R pipe, but the best PP-R pipe can be smashed even if the temperature is lower than 10 degrees. However, strong hardness does not mean good elasticity. Some manufacturers increase the hardness by adding too many impurities such as calcium carbonate, which cannot be broken, and are easily brittle after a long time; (due to the cold brittleness of PP-R raw materials, performance in several temperature ranges Different: 10, -5, -23...)

"burning" smoke smell

The PP-R tube with recycled plastic and other impurities mixed in the raw material will emit black smoke and have a pungent odor. And good materials will not emit black smoke and odor after burning, and the molten liquid is still very clean after burning. (Also you can "pull", see its pull "length")

"melt"

Den normale sveisetemperaturen til PP-R-rørledningen er i området 260-290 grader. Sveisekvaliteten vil være bedre garantert under sveising i dette temperaturområdet. Hvis sveiseparameterne er under normale sveiseparametere, kan produktet lett komme inn i sveisedysen under sveising. Og sveisehaugen er nær væske, det betyr at produktet ikke er produsert av autentiske PP-R-råmaterialer, og hvis sveisehaugen raskt kan avkjøles og herdes (vanligvis innen 10 sekunder), kan den også indikerer at produktet ikke er autentisk PP-R-råstoff Dette er fordi en av egenskapene til PP-R er at den termiske isolasjonseffekten er bedre, og kjølehastigheten vil naturlig nok være langsommere.

Sjekk om rørets indre diameter er deformert og om rørbeslagene er trukket. Et godt PP-R-rør kan ikke trekkes, og den indre diameteren blir ikke lett deformert.

"check"

Å låne testutstyr for testing kan effektivt skille fordeler og ulemper med produkter. Flere svært viktige testkrav er spesifisert i den nasjonale standarden, for eksempel aldringsmotstandstesten for rør (under ringspenningen på 1,9 MPa og testtemperaturen på 11 0 grader, testen som holder i 8760 timer uten feil) , stabilitetstesten av rørsystemet (varmt og kaldt) 5000 sykluser) og slagfasthetstest, etc., slik at brukeren kan be produsenten eller forretningsmannen om å gi testrapporten ovenfor for verifisering. I tillegg må det påpekes at den nasjonale standarden også har et viktig krav til råvarene som brukes til rør og rørdeler, som er smelteindeksen. Mer enn 0,5 g/10 min.